Artykuł w czasopiśmie
Brak miniatury
Licencja

CC-BYCC-BY - Uznanie autorstwa
 

Annealing-free fabrication of high-quality indium tin oxide films for free-carrier-based hybrid metal–semiconductor nanophotonics

dc.abstract.enRecent discoveries have revealed that indium tin oxide (ITO), due to the presence of an epsilon-near-zero (ENZ) point and suitable carrier concentration and mobility, can be used to modulate the refractive index, confine fields in the nanoscale, enhance nonlinear effects, achieve ultrafast light switching or to construct so-called time-varying media. While this potential positions ITO as a key material for future nanophotonic devices, producing ITO films with precisely engineered properties remains a significant challenge. Especially when the device’s complex geometry or incorporated materials require the fabrication process to be conducted at substrate temperatures below 100 °C and without any post-annealing treatment. Here we present a comprehensive study on the low-temperature deposition of 70 nm thick ITO films using an e-beam PVD system. The nanolayers evaporated under different conditions were characterized by SEM and AFM microscopy, Hall effect measurement system as well as spectroscopic ellipsometry. We discuss the factors influencing the optical, electrical, and morphological properties of ITO films. We show that smooth nanolayers of similar quality to annealed samples can be obtained at 80 °C by controlling the oxygen plasma parameters, and the ENZ wavelength can be tuned throughout the NIR spectral range. Finally, we show that using the proposed methodology, we fabricated ITO films with resistivity as low as 5.2 × 10–4 Ω cm, smooth surface with RMS < 1 nm, high carrier concentration reaching 1.2 × 1021 cm−3 and high transmittance (85%) in the Vis/NIR spectrum.
dc.affiliationUniwersytet Warszawski
dc.affiliation.departmentWydział Fizyki
dc.contributor.authorStefaniuk, Tomasz
dc.contributor.authorSzymczak, Julia
dc.contributor.authorKorneluk, Alexander
dc.date.accessioned2024-01-24T16:39:48Z
dc.date.available2024-01-24T16:39:48Z
dc.date.copyright2023
dc.date.issued2023
dc.description.abstract<jats:title>Abstract</jats:title><jats:p>Recent discoveries have revealed that indium tin oxide (ITO), due to the presence of an epsilon-near-zero (ENZ) point and suitable carrier concentration and mobility, can be used to modulate the refractive index, confine fields in the nanoscale, enhance nonlinear effects, achieve ultrafast light switching or to construct so-called time-varying media. While this potential positions ITO as a key material for future nanophotonic devices, producing ITO films with precisely engineered properties remains a significant challenge. Especially when the device’s complex geometry or incorporated materials require the fabrication process to be conducted at substrate temperatures below 100 °C and without any post-annealing treatment. Here we present a comprehensive study on the low-temperature deposition of 70 nm thick ITO films using an e-beam PVD system. The nanolayers evaporated under different conditions were characterized by SEM and AFM microscopy, Hall effect measurement system as well as spectroscopic ellipsometry. We discuss the factors influencing the optical, electrical, and morphological properties of ITO films. We show that smooth nanolayers of similar quality to annealed samples can be obtained at 80 °C by controlling the oxygen plasma parameters, and the ENZ wavelength can be tuned throughout the NIR spectral range. Finally, we show that using the proposed methodology, we fabricated ITO films with resistivity as low as 5.2 × 10<jats:sup>–4</jats:sup> Ω cm, smooth surface with RMS &lt; 1 nm, high carrier concentration reaching 1.2 × 10<jats:sup>21</jats:sup> cm<jats:sup>−3</jats:sup> and high transmittance (85%) in the Vis/NIR spectrum.</jats:p>
dc.description.financeNie dotyczy
dc.description.number1
dc.description.versionfinal_author
dc.description.volume13
dc.identifier.doi10.1038/S41598-023-45651-W
dc.identifier.issn2045-2322
dc.identifier.urihttps://repozytorium.uw.edu.pl//handle/item/100747
dc.identifier.weblinkhttps://doi.org/10.18150/N4KOSC
dc.languageeng
dc.pbn.affiliationphysical sciences
dc.relation.documents10.18150/N4KOSC
dc.relation.ispartofScientific Reports
dc.relation.pagesart. 18520
dc.rightsCC-BY
dc.sciencecloudnosend
dc.share.typeOPEN_JOURNAL
dc.titleAnnealing-free fabrication of high-quality indium tin oxide films for free-carrier-based hybrid metal–semiconductor nanophotonics
dc.typeJournalArticle
dspace.entity.typePublication
oaire.citation.issue1
oaire.citation.volume13